Product information for Greenville Tube 825 tubing
Super Austenitic 825 alloy provides strength resistance to oxidation and carburization.
| Grade |
OD |
Wall |
Lengths |
| 600 |
1/8" (3.18 mm) to 1-1/2" (38.1 mm) |
0.010"(0.25 mm) to 0.188" (4.78 mm) |
to 60' 6" (18.440 m) |
Composition of 800 tubing
| Grade |
825 |
| UNS Designation |
N08825 |
| Carbon (C) Max. |
1.5–3.0 |
| Manganese (Mn) Max. |
1.0 |
| Phosphorous (P) Max. |
— |
| Sulphur (S) Max. |
0.03 |
| Silicon (Si) Max. |
0.5 |
| Nickel (Ni) |
46.00 |
| Chromium (Cr) |
23.5 |
| Other Elements |
Iron 22.0 Min. |